Thermal stability of 1x10(20) cm(-3) Al+ implanted 4H-SiC after electrical activation at temperature >= 1850 degrees C
Contributo in Atti di convegno
Data di Pubblicazione:
2017
Abstract:
The effect of a 1500 degrees C treatment on 1x10(20) cm(-3) Al+ ion implanted in 4H-SiC samples that have been previously annealed at 1850-1950 degrees C is studied in this work. Up to 240 min annealing time at 1500 degrees C, the Al electrical activation reached at 1850-1950 degrees C is preserved.
Tipologia CRIS:
04.01 Contributo in Atti di convegno
Keywords:
doping by ion implantation; 4H-SiC
Elenco autori:
Puzzanghera, Maurizio; Canino, Mariaconcetta; Nipoti, Roberta
Link alla scheda completa:
Titolo del libro:
GALLIUM NITRIDE AND SILICON CARBIDE POWER TECHNOLOGIES 7
Pubblicato in: