abstract:
Erbium activated SiC/SiO2 nanocomposites doped with Er3+ concentrations ranging from 1 to 4 mol% were prepared by pyrolysis of sol¨Cgel derived precursors. The gels were obtained from modified silicon alkoxides containing Si¨CCH3 and Si¨CH groups. Thin discs obtained from the monolithic xerogels were pyrolyzed in an alumina tubular furnace in flowing Ar (100 ml/min) at 800, 1000, 1200 and 1300 ¡ãC. The samples were investigated by absorption and photoluminescence spectroscopies. Emission in the C-telecommunication band was observed at room temperature for all the samples upon continuous-wave excitation at 980 or 514.5 nm. The shape of the emission band corresponding to the 4I13/2 ¡ú 4I15/2 transition is found to be independent both on Erbium content and excitation wavelength, with a FullWidth Half Maximum (FWHM) of 48 nm. By increasing the pyrolysis temperature the intensity of the luminescence increases and the electronic bandgap energy decreasesErbium activated SiC/SiO2 nanocomposites doped with Er3+ concentrations ranging from 1 to 4 mol% were prepared by pyrolysis of sol¨Cgel derived precursors. The gels were obtained from modified silicon alkoxides containing Si¨CCH3 and Si¨CH groups. Thin discs obtained from the monolithic xerogels were pyrolyzed in an alumina tubular furnace in flowing Ar (100 ml/min) at 800, 1000, 1200 and 1300 ¡ãC. The samples were investigated by absorption and photoluminescence spectroscopies. Emission in the C-telecommunication band was observed at room temperature for all the samples upon continuous-wave excitation at 980 or 514.5 nm. The shape of the emission band corresponding to the 4I13/2 ¡ú 4I15/2 transition is found to be independent both on Erbium content and excitation wavelength, with a FullWidth Half Maximum (FWHM) of 48 nm. By increasing the pyrolysis temperature the intensity of the luminescence increases and the electronic bandgap energy decreases
Iris type:
01.01 Articolo in rivista
Keywords:
FWHM; 4I13/2; Emission band
List of contributors:
Ferrari, Maurizio
Handle:
https://iris.cnr.it/handle/20.500.14243/20945
Published in:
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY
Journal
  • Use of cookies

Powered by VIVO | Designed by Cineca | 26.5.0.0 | Sorgente dati: PREPROD (Ribaltamento disabilitato)